Superalloy resources
Read Online
Share

Superalloy resources supply and availability by Joseph R. Stephens

  • 346 Want to read
  • ·
  • 28 Currently reading

Published by National Aeronautics and Space Administration, For sale by the National Technical Information Service in [Washington, DC, Springfield, Va .
Written in English

Subjects:

  • Heat resistant alloys.

Book details:

Edition Notes

StatementJoseph R. Stephens.
SeriesNASA technical memorandum -- 89866.
ContributionsUnited States. National Aeronautics and Space Administration.
The Physical Object
FormatMicroform
Pagination1 v.
ID Numbers
Open LibraryOL15284063M

Download Superalloy resources

PDF EPUB FB2 MOBI RTF

Superalloys are unique high-temperature materials used in gas turbine engines, which display excellent resistance to mechanical and chemical degradation. This book presents the underlying metallurgical principles which have guided their development and practical aspects of component design and fabrication from an engineering by: COVID Resources. Reliable information about the coronavirus (COVID) is available from the World Health Organization (current situation, international travel).Numerous and frequently-updated resource results are available from this ’s WebJunction has pulled together information and resources to assist library staff as they consider how to handle coronavirus. The present work covers the development history of superalloys, the supply status and availability of strategic materials associated with superalloy compositions, primary and secondary melt processing for superalloys, the metallurgy of investment-cast superalloy components, the nature and properties of single-crystal superalloys, the thermomechanical processing of superalloys, and the effects of .   Superalloys are unique high-temperature materials used in gas turbine engines, which display excellent resistance to mechanical and chemical degradation. This book /5(4).

Abstract: The following sections are included: INTRODUCTION. COMPOSITION AND MICROSTRUCTURE. The Gamma Matrix (γ) Gamma Prime. Gamma Double Prime. Carbides. Amazon Inspire Digital Educational Resources: Amazon Rapids Fun stories for kids on the go: Amazon Web Services Scalable Cloud Computing Services: Audible Listen to Books & Original Audio Performances: Book Depository Books With Free Delivery Worldwide: Box Office Mojo Find Movie Box Office Data: ComiXology Thousands of Digital Comics. No part of this book may be reproduced, stored in a retrieval system, or transmitted, in any form or by any means, electronic, mechanical, photocopying, recording, or otherwise, without the written permission of the copyright owner. First printing, March Great care is taken in the compilation and production of this book, but it should be. All the different aspects of the processing and properties of superalloys, including monocrystals, are systematically set out in chapters of an impressive book (Tien and Caulfield ).

  Development of a Low‐Density Rhenium‐Free Single Crystal Nickel‐Based Superalloy by Application of Numerical Multi‐Criteria Optimization Using . Home» Publications» Proceedings & Other Resources» Superalloys Proceedings Archive. Superalloys Proceedings Archive. The Superalloys Conference Proceedings Archive offers an online collection of more than 1, technical articles that document the history of these important materials, starting with the International Symposium on the. ASM International, - Heat resistant alloys - pages 5 Reviews This book covers virtually all technical aspects related to the selection, processing, use, and analysis of superalloys. The 4/5(5). Superalloys have been defined many times by metallurgists for books and conferences, with reasonable consistency. A few of the most comprehensive definitions follow: 1. A superalloy, or high-performance alloy, is an alloy usually based on Group VIII A.